Plasticizing

Rotating of melt

Back pressure improves plasticizing

Dosing

Deactivating, if the required volume is in front of the screw      

Injection

Axial movement of the screw forward à injection of melt      

Switch over from “injection pressure” to “hold pressure”

(compensation of PET- der PET-Shrinkage)      

Cooling

Deactivation of  Holding Pressure = Start Cooling

Nozzles close

Melt for the next injection cycle is plasticized

End of Cooling time is, when the preform wall temperature is <70 °C Ejection Mold opens Preforms are ejected by the ejection pins Mold closes Next injection molding can start Mold structure / assembly Mold Cycle Time (Single Step) - Preform 26,5g (Standard Plasticizing: 12 g/sec) [/av_textblock] [/av_one_full]